Transverse impact of circular marine composite plates

Authors: Sutlierland, L.S. Guedes Soares

ABSTRACT:

Falling-weight impact tests on circular low fibre-volume E-glass/polyester composite plates have been performed. Three behaviour regimes have been defined: 'Undelaminated', 'Delaminated' and 'Fibre damage'. A fracture mechanics model describes extremely well the sudden onset of delamination, and gives good scaling between specimen sizes. Bending and membrane effects are significant for thin laminates. For thick laminates, especially after the sudden onset of delamination, the response is well described by an energy balance model strains.

Key Words:
Affiliation:

Sutlierland1| L.S. Guedes Soares2

1 Bolseiro de Pés-Doutoramento, 2 Prof. Catedrático, Unidade de Engenharia e Tecnologia Naval, IST, Lisboa, Portugal